FireDOC Search

Author
Kiang, J. K. Y. | Uden, P. C. | Chien, J. C. W.
Title
Polymer Reactions. Part 7. Thermal Pyrolysis of Poly(Isoprene).
Coporate
Massachusetts Univ., Amherst
Sponsor
National Institute of Standards and Technology, Gaithersburg, MD
Report
Part 7, no date, 27 p.
Contract
NBS-GRANT-G7-9010
Keywords
pyrolysis | polypropylene | flash pyrolysis
Abstract
Poly(propylene) has been pyrolyzed in a carrier stream of helium from 388 deg to 900 deg C in both programmed heating and flash pyrolysis modes. The products were on-line identified and quantitatively analyzed by an interfaced GC peak identification system. The first order rate constants for pyrolysis are 3.7 x 10(-4) sec.(-1) and 4.0 x 10(-4) sec.(-1), respectively, for atactic and isotactic poly(propylene) at 388 deg C; the corresponding overall activation energies are 56 ±6 and 51 ±5 kcal. mole(-1). The main products in decreasing yields are 2,4-dimethyl-l-heptene, 2-pentene, propylene, 2 methyl-l-pentene, and 2,4,6-trimethyl-l-nonene.