FireDOC Search

displaying 1 - 10 results in total 12

  • Masarik, I.; Svetlik, J.; Horak, Z.
    view article (1.0)

    Thermo-oxidative Decomposition, Ignition and Burning of Flame-Retarded Polystyrenes.
    Fire Research Lab., Prague, Czechoslovakia; Czechoslovak Academy of Sciences, Prague; Kaucuk Kralupy k.p., Czechoslovakia
    Fire and Materials, Vol. 6, No. 2, 59-64, June 1982

  • Michal, J.; Mitera, J.; Tardon, S.
    view article (1.0)

    Toxicity of Thermal Degradation Products of Polyethylene and Polypropylene.
    Ore Research Institute, Praha, Czechoslovakia; Institute of Chemical Technology, Praha, Czechoslovakia; Coal Research Institute, Ostrava-Radvanice, Czechoslovakia
    Fire and Materials, Vol. 1, No. 4, 160-180, December 1976

  • Masarik, I.; Ryska, M..; Svetlik, J.; Horak, Z.
    view article (1.0)

    Use of the Setchkin Apparatus--Mass Spectrometry in the Investigaiton of Ignition and Burning of Flame Retarded Polystyrenes.
    Fire Research Lab., Praha, Czechoslovakia; Institute of Macromolecular Chemical Prague, Czechoslovakia; Research Institute of Synthetic Rubber, Kralupy, Czechoslovakia
    Fire and Materials, Vol. 1, No. 4, 129-133, December 1976

  • Kosik, M.; Luzakova, V.; Reiser, V.; Blazej, A.
    view article (1.0)

    Thermal Degradation and Flammability of Cellulosics.
    Slovak Technical University, Bratislava, Czechoslavakia
    Fire and Materials, Vol. 1, 19-23, March 1976

  • Qianwei, X.; Jinwang, R.
    view article (1.0)

    Study on Flame Retardation Mechanisms of Al2O3-3H2O and Mg(OH)2 by Thermal Analysis.
    Tong Ji Univ., Shanghai, China
    China Ordnance Society. International Symposium on Flame Retardants Proceedings. November 1-5, 1989, International Academic Publishers, Beijing, China, Yuxiang, O. and Minxiu, Z., Editors, 332-336 p., 1989

  • Metcalfe, E.; Harman, A. R.; Patel, M. K.
    view article (1.0)

    Thermo-Oxidative Degradation of PTFE in the NIST Cup Furnace Toxicity Test.
    Thames Polytechnic, London, England
    Fire and Materials, Vol. 15, No. 2, 53-58, April/June 1991

  • Nielsen, C. A.; Pierini, P.; Fuh, S.
    view article (1.0)

    Thermal and Thermo-Oxidative Degradation of PBO: Determination of Kinetics and Reaction Products.
    Dow Chemical, Walnut Creet, CA
    Journal of Fire Sciences, Vol. 11, No. 2, 156-171, March/April 1993
    Sagamore Army Materials Research Conference, 39th. September 16-17, 1992, Plymouth, MA, ['1992', '1993']

  • Cicchetti, O.; Bertelli, G.; Bevilacqua, A.; Cipolli, R.; Pagliari, A.
    view article (1.0)

    Advances in Intumescent Flame Retardant Additive Technology.
    Himont, Milano, Italy
    British Plastics Federation AND Institute of Materials. Flame Retardants '94. International Conference, 6th. January 26-27, 1994, Interscience Communications Ltd., London, England, London, England, 129-142 p., 1994

  • Bourbigot, S.; Richard-Campisi, L.; LeBras, M.; Delobel, R.
    view article (1.0)

    Thermal Behavior of a Blend of Cotton and Fire-Retardant Polyester Fibers: A Kinetic Study.
    Universite des Sciences et Technologies de Lille, France; C.R.E.P.I.M., Bully les Mines, France
    Journal of the Textile Institute, Vol. 88, No. 1, 4-75, 1997

  • Sinden, D. P.; Anand, S.; Kandola, B.; Horrocks, R.
    view article (1.0)

    Multivariate Analysis of the Performance of Responsive Heat Barrier Materials.
    Bolton Institute, UK
    Polymer International, Vol. 49, No. 10, 1226-1231, October 10, 2000