Braun, D.
view article (6.2724433)
Thermal Degradation of Poly(Vinyl Chloride).
Deutsches Kunststoff-Institut, Darmstadt, West Germany
Developments in Polymer Degradation. Volume 3,
Applied Science Publishers Ltd., Essex, England,
101-133 p.,
1981
Kubin, R. F.
view article (6.2724433)
Thermal Characteristics of 3501-6/AS and 5208/T300 Graphite Epoxy Composites.
Naval Weapons Center, China Lake, CA
NWC-TP-6104,
May 1979,
18 p.
Michal, J.
view article (6.2724433)
Combustion Products of Polymeric Materials. Part 2. Test Chamber CAB 650.
Ore Research Inst., Prague, Czechoslovakia
Fire and Materials,
Vol. 7,
No. 4,
169-172,
1983
Zitting, A.; Heinonen, T.
view article (6.2724433)
Decrease of Reduced Glutathione in Isolated Rat Hepatocytes Caused by Acrolein, Acrylonitrile, and the Thermal Degradation Products of Styrene Copolymers.
Institute of Occupational Health, Helsinki, Finland
Toxicology,
Vol. 17,
333-341,
1980
Vovelle, C.; Akrich, R.; Mellotte, H.
view article (6.2724433)
Thermal Degradation of Painted Wood. An Experimental Study.
Centre de Recherches sur la Chimie de la Combustion, Orleans, France
Journal of Fire Sciences,
Vol. 1,
No. 3,
191-199,
May/June 1983
Birky, M. M.
view article (6.2724433)
Review of Smoke and Toxic Gas Hazards in Fire Environment.
National Bureau of Standards, Gaithersburg, MD
CIB W14/26/75 (USA),
University of Edinburgh Centre for Industrial Consultancy and Liaison with the Department of Fire Safety Engineering. Fire Safety of Combustible Materials. International Symposium. October 1975, CIB W14/26/75 (USA), England, 231-252 pp, 1975 AND U.S./Japan Government Cooperative Program on Natural Resources (UJNR). Panel on Fire Research and Safety. Volume 1. Toxicity. October 19-22, 1976, TH9127.J2U58 1976, Tokyo, Japan, 1-23 pp, 1976,
England,
1976
Fung, D. P. C.
view article (6.2724433)
Kinetics and Mechanism of the Thermal Degradation of Cellulose.
Forest Products Lab., Ottawa, Canada
Technical Association of the Pulp Paper Industry,
Vol. 52,
No. 2,
319-321,
February 1969
Schiltz, R. J.
view article (6.2724433)
Investigation of the Structural Degradation and Personnel Hazards Resulting From Helicopter Composite Structures Exposed to Fires and/or Explosions. Final Report. March 1979-December 1980.
Bell Helicopter Textron, Forth Worth, TX
Army Research and Technology Labs., Fort Eustis, VA,
USAAVRADCOM-TR-81-D-16,
August 1981,
110 p.
Brauman, S. K.
view article (6.2724433)
Char Formation in Polyvinyl Chloride. Part 2. Influence of the Charring Agent Zinc Pyromellitate on the Thermal Degradation of PVC During Radiant Pyrolysis.
SRI International, Menlo Park, CA
Journal of Fire Retardant Chemistry,
Vol. 7,
No. 4,
175-182,
November 1980
Inagaki, N.; Goto, K.; Katsuura, K.
view article (6.2724433)
Thermal Degradation of Poly(diethyl vinylphosphonate) and Its Copolymer.
Shizuoka Univ., Japan
Polymer,
Vol. 16,
641-644,
September 1975