Koziowski, R.; Wesolek, D.; Muzyczek, M.
view article (6.408976)
Toxic Products of Thermal Deterioration and Combustion of Wood-Based and Textile Materials.
Institute of Natural Fibers, Poznan, Poland
China Ordnance Society. International Symposium on Flame Retardants Proceedings. November 1-5, 1989,
International Academic Publishers,
Beijing, China,
Yuxiang, O. and Minxiu, Z., Editors,
689-697 p.,
1989
Ehlers, G. F. L.; Fisch, K. R.; Powell, W. R.
view article (6.408976)
Studies of the Breakdown Mechanism of Polymers. Part 7. The Thermal Decomposition of a Polyhydrazide and of Polyoxadiazoles.
Air Force Materials Lab., Wright-Patterson AFB, OH
AFML-TR-72-67,
April 1972,
34 p.
Popov, L. A.; Yablochkin, V. D.
view article (6.408976)
Characteristics of Gases Released by Polyvinyl Chloride Film.
Institute for Medico-Biological Research of the Ministry of Health, USSR
Hygiene and Sanitation,
Vol. 32,
114-117,
1967
Einhorn, I. N.; Chatfield, D. A.; Futrell, J. H.; Mickelson, R. W.; Voorhees, K. J.; Hileman, F. D.; Ryan, P. W.
view article (6.408976)
Methodology for the Analysis of Combustion Products.
Utah Univ., Salt Lake City
FRC/UU-49; UTEC 75-073,
University of Utah. Flammability of Materials. Polymer Conference Series. July 7-11, 1975,
Salt Lake City, UT,
1-56 p.,
1975
Pommersheim, J. M.; Clifton, J. R.
view article (6.408976)
Models of Transport Processes in Concrete.
National Institute of Standards and Technology, Gaithersburg, MD; Bucknell Univ., Lewisburg, PA
Nuclear Regulatory Commission, Washington, DC,
NISTIR 4405,
September 1990,
101 p.
Dean, L.; Groves, S.; Hancox, R.; Lamb, G.; Lehrle, R. S.
view article (6.408976)
Pyrolysis-GC and MS Applied to Study Oligomer Formation in the Degradation of Polystyrene and Styrene Copolymers.
Brimingham Univ., UK
Polymer Degradation and Stability,
Vol. 25,
No. 2-4,
143-160,
1989
Kashiwagi, T.; Nambu, H.
view article (6.408976)
Global Kinetic Constants for Thermal Oxidative Degradation of a Cellulosic Paper.
National Institute of Standards and Technology, Gaithersburg, MD
Combustion and Flame,
Vol. 88,
No. 3-4,
345-368,
1992
National Aeronautics and Space Administration, Lewis Research Center, Cleveland, OH,
Combustion Institute/Eastern Section. Chemical and Physical Processes in Combustion. Proceedings. Fall Technical Meeting, 1991. October 14-16, 1991,
Ithaca, NY,
91/1-4 p.,
['1991', '1992']
Jolles, Z. E.; Jolles, G. I.
view article (6.408976)
Some Notes on Flame-Retardant Mechanisms in Polymers.
Paper 10,
Plastics Institute. Plastics in Fire Conference. November 2-3, 1971,
London, England,
1-19 p.,
1971
Nichols, J. R.; Lipska, A. E.
view article (6.408976)
Analytical Gas Chromatograph for Products of Isothermally Degraded Polymers.
Naval Radiological Defense Lab., San Francisco, CA
USNRDL-TR-68-413; OCD Work Unit 2531C,
February 5, 1968,
45 p.
Nowlen, S. P.; Jacobus, M. J.
view article (6.408976)
Estimation of Electrical Cable Fire-Induced Damage Limits.
Sandia National Labs., Albuquerque, NM
Interscience Communications Limited. Fire and Materials. International Conference, 1st. September 24-25, 1992,
Arlington, VA,
213-222 p.,
1992