FireDOC Search

displaying 301 - 310 results in total 311

  • Dodd, A. B.; Lautenberger, C.; Fernandez-Pello, A. C.
    view article (1.0)

    Numerical Examination of Two-Dimensional Smolder Structure in Polyurethane Foam.
    Sandia National Laboratories, Albuquerque, NM; California Univ., Berkeley
    Volume 32; Part 2,
    Combustion Institute, Symposium (International) on Combustion, 32nd. Proceedings. Volume 32. Part 2. August 3-8, 2008, Combustion Institute, Pittsburgh, PA, Montreal, Canada, Dagaut, P.; Sick, V., Editors, 2497-2504 p., 2009

  • Konig, A.; Fehrenbacher, U.; Kroke, E.; Hirth, T.
    view article (1.0)

    Thermal Decomposition Behavior of the Flame Retardant Melamine in Slabstock Flexible Polyurethane Foams.
    Fraunhofer-Institut für Chemische Technologie, ICT, 76327 Pfinztal, Germany; Technische Universitaet Bergakademie Freiberg, 09596 Freiberg, Germany; Fraunhofer-Institut für Grenzflächen- und Bioverfahrenstechnik IGB, 70569 Stuttgart, Germany
    Journal of Fire Sciences, Vol. 27, No. 3, 187-211, May 2009

  • Huang, N.; Wang, J.
    view article (1.0)

    Studies of the Action of Silicone at the Interphase on the Flame Retardant System of EBA Copolymer-Chalk.
    Wuhan University of Science and Engineering, Hu Bei Province, China; Beijing Institute of Technology, 100081 Beijing, China
    Journal of Fire Sciences, Vol. 27, No. 3, 235-264, May 2009

  • Zhang, J.; Hereid, J.; Hagen, M.; Bakirtzis, D.; Delichatsios, M. A.; Fina, A.; Castrovinci, A.; Camino, G.; Samyn, F.; Bourbigot, S.
    view article (1.0)

    Effects of Nanoclay and Fire Retardants on Fire Retardancy of a Polymer Blend of EVA and LDPE.
    Ulster Univ., Newtownabbey, BT37 0QB, UK; Politecnico di Torino, 15100 Alessandria, Italy; Procédés d'Elaboration de Revêtements Fonctionnels (PERF), 59650 Villeneuve d'Ascq, France
    Combustion and Flame, Vol. 156, No. 5, 504-513, May 2009

  • Fall, M.; Samb, S. S.
    view article (1.0)

    Effect of High Temperature on Strength and Microstructural Properties of Cemented Paste Backfill.
    Ottawa Univ., Ontario, Canada K1N 6N5
    Fire Safety Journal, Vol. 44, No. 4, 642-651, May 2009

  • He, Q.; Lu, H.; Song, L.; Hu, Y.; Chen, L.
    view article (1.0)

    Flammability and Thermal Properties of a Novel Intumescent Flame Retardant Polypropylene.
    University of Science and Technology of China, Hefei, Anhui 230026, P.R. China
    Journal of Fire Sciences, Vol. 27, No. 4, 303-321, July 2009

  • Chen, X.; Jiao, C.
    view article (1.0)

    Synergistic Effects of Hydroxy Silicone Oil on Intumescent Flame Retardant Polypropylene System.
    Qingdao University of Science and Technology, Qingdao, Shandong 266042, PR China
    Fire Safety Journal, Vol. 44, No. 8, 1010-1014, November 2009

  • Bakirtzis, D.; Ramani, A.; Delicatsios, M. A.; Zhang, J.
    view article (1.0)

    Structure of the Condensed Phase and Char of Fire-Retarded PBT Nanocomposites by TGA/ATR in N2.
    Ulster University, BT37 0QB, UK
    Fire Safety Journal, Vol. 44, No. 8, 1023-1029, November 2009

  • Hagen, M.; Hereid, J.; Delichatsios, M. A.; Zhang, J.; Bakirtzis, D.
    view article (1.0)

    Flammability Assessment of Fire-Retarded Nordic Spruce Wood Using Thermogravimetric Analyses and Cone Calorimetry.
    University of Ulster, Northern Ireland
    Fire Safety Journal, Vol. 44, No. 8, 1053-1066, November 2009

  • Gong, X.; Guo, Z.; Wang, Z.
    view article (1.0)

    Reactivity of Pulverized Coals During Combustion Catalyzed by CeO2 and Fe2O3.
    Chinese Academy of Sciences, Beijing, China; China Graduate University of Chinese Academy of Sciences, Beijing, China; University of Science and Technology, Beijing, China
    Combustion and Flame, Vol. 157, No. 2, 351-356, February 2010